Size
350 × 2.5 × 40 mm
Steel
HSS M2 (DMo5)
Best for
Mild steel tube, solid bar and profiles
Machine
Cold saws for 350 mm blades with a 40 mm arbor
Quantity bands
50–199 · 200–999 · 1,000–5,000 · 5,000+ pcs
Size
350 × 2.5 × 40 mm
Steel
HSS M2 (DMo5)
Best for
Mild steel tube, solid bar and profiles
Machine
Cold saws for 350 mm blades with a 40 mm arbor
Quantity bands
50–199 · 200–999 · 1,000–5,000 · 5,000+ pcs

Choose the tooth pitch

As a rule, at least two or three teeth should be in the cut at the same time. Thin-wall tube needs fine teeth. Solid bar and thick sections need coarse teeth, so the gullets have room for the chips. With too few teeth in the cut, teeth catch and break. With too many, the chips pack in and the blade overheats.

What the thickness means

A 2.5 mm blade is a common middle choice. It is stable enough for solid bar and heavier profiles, with a moderate kerf.

Run in a new blade

Make the first cuts with a reduced feed. This gently hones the new cutting edges and helps the blade last longer. Then raise the feed step by step to your normal setting.

Speed, feed and coolant

  • Speed

    HSS cold saws run slowly. Harder steel and stainless steel need a lower speed than mild steel.

  • Feed

    Even chips with a light colour show a good feed. Blue chips mean too much heat.

  • Coolant

    Use cutting fluid at the right mix, aimed at the teeth, so it cools and washes out the chips.

  • Speed

    HSS cold saws run slowly. Harder steel and stainless steel need a lower speed than mild steel.

  • Feed

    Even chips with a light colour show a good feed. Blue chips mean too much heat.

  • Coolant

    Use cutting fluid at the right mix, aimed at the teeth, so it cools and washes out the chips.

When to resharpen

  • A growing burr on the cut end

  • The cut runs out of square

  • More noise, vibration or force than usual

  • A growing burr on the cut end

  • The cut runs out of square

  • More noise, vibration or force than usual

Resharpen early and keep the original tooth shape. Each resharpening makes the diameter a little smaller, so check that the blade still reaches through your largest section.

Send these details for your bulk quotation

  • Teeth

    Number of teeth or the pitch, and the tooth shape

  • Pin holes

    The pattern, or your machine make and model

  • Material

    What you cut, with the tube wall or bar size

  • Coating

    Uncoated, or ask for TiN / TiAlN

  • Quantity

    Your band, and one-off or repeat order

  • Teeth

    Number of teeth or the pitch, and the tooth shape

  • Pin holes

    The pattern, or your machine make and model

  • Material

    What you cut, with the tube wall or bar size

  • Coating

    Uncoated, or ask for TiN / TiAlN

  • Quantity

    Your band, and one-off or repeat order

No drawing? A phone photo of the blade you use now, with a ruler beside it, is enough to start.

Why do the teeth break?

The usual causes are too few teeth in the cut, a loose clamp, or too high a feed. Check these before you change the blade type.

What is the smallest order?

This page is for bulk orders from 50 pcs. If you need fewer, say so in the form and our team will tell you what is possible.

How is the price set?

The price depends on the size, the steel, the teeth, any coating and the quantity band. You receive a written quotation before you order.

Section
Cold Saw Blades
Updated
19 November 2026
Reading time
3 min read

Ready to order in volume?

Orders from 50 to 5,000+ pieces. Send your size or drawing and the quantity, and our team replies with a quotation.

Request a volume quote